A4.5M/A4.5:2020 (ISO 15792-3:2011 MOD) STANDARD METHODS FOR CLASSIFICATION TESTING OF POSITIONAL CAPACITY AND ROOT PENETRATION OF WELDING CONSUMABLES IN A FILLET WELD



Member Price: $63.00

Non-Member Price: $84.00

This standard describes preparation and assessment of a fillet weld test piece. Test conditions prescribed and results required should not be considered to be requirements or expectations for a procedure qualification. This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other. ISBN Print: 978-1-64322-103-8 ISBN PDF: 978-1-64322-104-5