AWS-NAVSEA B2.1-1-313:2020 STANDARD WELDING PROCEDURE SPECIFICATION FOR NAVAL APPLICATIONS (SWPS-N) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL (S-1), 1/8 INCH [3 MM] THROUGH 1-1/2 INCH [38 MM] THICK, MIL- 70S-2 AND MIL-7018-M
Member Price: $264.00
Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc welding followed by shielded metal arc
welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and joint designs for groove and fillet welds. This SWPS-N was developed primarily for naval applications that
require performance to NAVSEA Technical Publication S9074-AQ-GIB-010/248, Requirements for Welding and Brazing Procedure and Performance Qualification. ISBN Print: 978-1-64322-107-6 ISBN PDF: 978-1-64322-108-3