Picture of AWS B2.1-4-220:2021 - Standard Welding Procedure Specification (SWPS) for Gas Tungsten Arc Welding (Consumable Insert Root) of Chromium- Molybdenum Steel (M-4/P-4, Group 1 or 2), IN515

AWS B2.1-4-220:2021 - Standard Welding Procedure Specification (SWPS) for Gas Tungsten Arc Welding (Consumable Insert Root) of Chromium- Molybdenum Steel (M-4/P-4, Group 1 or 2), IN515



Member Price: $228.00

Non-Member Price: $304.00

This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 in. through 3/4 in. in the postweld heat treated (PWHT) condition, using manual gas tungsten arc welding with a consumable insert root. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This welding procedure specification (WPS) was developed primarily for pipe applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$228.00
$304.00
Download PDF
$228.00
$304.00