Picture of B2.1-1-234:2020-AMD1 - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 75% ARGON PLUS 25% CARBON DIOXIDE SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL , IN THE AS-WELDED OR PWHT CONDITION, PRIMARILY PIPE APPLICATIONS (2ND PRINTING)

B2.1-1-234:2020-AMD1 - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 75% ARGON PLUS 25% CARBON DIOXIDE SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL , IN THE AS-WELDED OR PWHT CONDITION, PRIMARILY PIPE APPLICATIONS (2ND PRINTING)



Member Price: $246.00

Non-Member Price: $328.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using 75% argon plus 25% carbon dioxide shielded flux cored arc welding. It cites the base metals
and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove and fillet welds. This SWPS was developed primarily for pipe applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$246.00
$328.00
Download PDF
$246.00
$328.00