Picture of AWS B2.1-1-027:2018(R2022) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1 or P-1, GROUP 1 OR 2), 1/8 INCH [3 MM] THICK, E71T-11, AS-WELDED CONDITION, PRIMARILY PLATE AND STRUCTURAL APPLICATIONS

AWS B2.1-1-027:2018(R2022) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1 or P-1, GROUP 1 OR 2), 1/8 INCH [3 MM] THICK, E71T-11, AS-WELDED CONDITION, PRIMARILY PLATE AND STRUCTURAL APPLICATIONS



Member Price: $246.00

Non-Member Price: $328.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1/2 inch [13 mm], using self-shielded flux cored arc welding. It cites the base metals and operating conditions necessary
to make the weldment, the filler metal specifications, and the allowable joint designs for groove and fillet welds. This SWPS was developed primarily for plate and structural applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$246.00
$328.00
Download PDF
$246.00
$328.00