D14.0/D14.0M:2024 - MACHINERY AND EQUIPMENT WELDING SPECIFICATION



Member Price: $186.00

Non-Member Price: $248.00

This specification establishes design, manufacture, quality, inspection, and repair requirements for carbon, low-alloy, and alloy steel welded connections in machinery and equipment. It addresses topics including weld joint design, workmanship,
quality acceptance criteria, nondestructive examination methods (visual, radiographic, ultrasonic, magnetic particle, and liquid penetrant), repair of weld defects, and postweld heat treatment.