Picture of C3.12M/C3.12:2024 SPECIFICATION FOR FURNACE SOLDERING

C3.12M/C3.12:2024 SPECIFICATION FOR FURNACE SOLDERING



Member Price: $66.00

Non-Member Price: $88.00

This specification provides the minimum requirements for equipment, materials, processing procedures as well as inspection for metal and ceramic base materials that can be furnace soldered. This specification provides criteria for classifying furnace soldered joints based on loading and the consequences of failure. It also provides quality assurance criteria that define the limits of acceptability in each class. This specification describes acceptable furnace soldering equipment, materials, and procedures, as well as the required inspection for each class of solder joint so produced. ISBN: 978-0-87171-913-3

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$66.00
$88.00
Download PDF
$66.00
$88.00