Picture of AWS-NAVSEA B2.1-1-302:2015 (R2025) - STANDARD WELDING PROCEDURE SPECIFICATION FOR NAVAL APPLICATIONS (SWPS-N) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL (S-1), 1/8 INCH [3 MM] THROUGH 1-1/2 INCH [38 MM] THICK, MIL-7018-M, IN THE AS-WELDED OR PWHT CONDITION

AWS-NAVSEA B2.1-1-302:2015 (R2025) - STANDARD WELDING PROCEDURE SPECIFICATION FOR NAVAL APPLICATIONS (SWPS-N) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL (S-1), 1/8 INCH [3 MM] THROUGH 1-1/2 INCH [38 MM] THICK, MIL-7018-M, IN THE AS-WELDED OR PWHT CONDITION



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through
1-1/2 inch [38 mm], using manual shielded metal arc welding. It cites the base metals and operating conditions necessary
to make the weldment, the filler metal specifications, and joint designs for groove and fillet welds. This SWPS-N was
developed primarily for naval applications that require performance to NAVSEA Technical Publication S9074-AQGIB-
010/248, Requirements for Welding and Brazing Procedure and Performance Qualification.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00