A5.14/A5.14M:2026 - SPECIFICATION FOR NICKEL AND NICKEL-ALLOY BARE WELDING ELECTRODES AND RODS
Member Price: $69.00
Non-Member Price: $92.00
The chemical compositions of nickel and nickel-alloy welding electrodes and rods are specified. Major topics include general requirements, testing, packaging, and application guidelines.
This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other.