This code covers the arc and braze welding requirements for nonstructural sheet metal fabrications using the commonly welded metals available in sheet form. Requirements and limitations governing procedure and performance qualification are presented, and workmanship and inspection standards are supplied. The informative annexes provide useful information on materials and processes.