Picture of G1.10M:2001 GUIDE FOR THE EVALUATION OF HOT GAS, HOT GAS EXTRUSION, AND HEATEDTOOL BUTT THERMOPLASTIC WELDS (HISTORICAL)

G1.10M:2001 GUIDE FOR THE EVALUATION OF HOT GAS, HOT GAS EXTRUSION, AND HEATEDTOOL BUTT THERMOPLASTIC WELDS (HISTORICAL)



Member Price: $56.00

Non-Member Price: $74.00

This guide lists and describes defects in welded joints in thermoplastic materials, and classifies each into one of three quality grades, allowing specific defects to be excluded or kept within limits. ISBN 0-87171-615-1