G1.2M/G1.2:1999 SPECIFICATION FOR STANDARDIZED ULTRASONIC WELDING TEST SPECIMEN FOR THERMOPLASTICS (HISTORICAL)
Member Price: $48.00
Non-Member Price: $64.00
You need this document to help minimize variations in the geometry, welding, and testing of the ultrasonic welding test sample for thermoplastics. Detailed figures show tolerances on critical dimensions that may affect weldability. Use this specification for studies on the ultrasonic welding of thermoplastics, weldability studies, and optimizations. ANSI Approved. ISBN 0-87171-585-6