D8.9:2002 RECOMMENDED PRACTICES FOR TEST METHODS FOR EVALUATING THE RESISTANCE SPOT WELDING BEHAVIOR OF AUTOMOTIVE SHEET STEEL MATERIALS (HISTORICAL)



Member Price: $63.00

Non-Member Price: $84.00

Helps to predict the performance of sheet steel that is resistance spot welded for use in auto manufacturing. Also addresses equipment setup, electrode installation and dressing, electrode endurance testing, and current level and range assessment. ANSI Approved. 78 pages, 3 annexes, 30 figures, 12 tables, softbound. 8 12 x 11, 2002. mouse. ISBN 0-87171-672-0