A5.32/A5.32M:1997 SPECIFICATION FOR WELDING SHIELDING GASES (HISTORICAL)
Member Price: $66.00
Non-Member Price: $88.00
This specification for welding shielding gases specifies minimum requirements for the composition and purity of the most popular single-component shielding gases. Classification designators for both single and multicomponent gases are introduced. Other topics include testing procedures, package marking, and general application guidelines. This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other. ANSI Approved. approx. 20 pages ISBN 0-87171-523-6 Historical See AWS A5.32/A5.32M (R2007)