D17.2/D17.2M:2007 SPECIFICATION FOR RESISTANCE WELDING FOR AEROSPACE APPLICATIONS (HISTORICAL)
Member Price: $48.00
Non-Member Price: $64.00
Requirements for aerospace resistance spot and seam welding of aluminum, magnesium, steel, nickel, cobalt, titanium, and their alloys. Intended to replace MIL-W-6858D and AMS-W- 6858A. ANSI Approved. approx. 44 pages,11 figures, 13 tables. ISBN 978-0-87171-064-2