Picture of A5.16/A5.16M:2007 SPECIFICATION FOR TITANIUM AND TITANIUM-ALLOY WELDING ELECTRODES AND RODS (HISTORICAL)

A5.16/A5.16M:2007 SPECIFICATION FOR TITANIUM AND TITANIUM-ALLOY WELDING ELECTRODES AND RODS (HISTORICAL)



Member Price: $63.00

Non-Member Price: $84.00

AWS A5.16/A5.16M:2007 is a revision of the titanium welding electrode document last revised in 2004. The compositions specified for each classification represent the state of the art. The specification contains testing procedures, standard sizes and forms, and identification and marking practices. This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other. ISBN 978-0-87171-077-2

Formats Member Price Non-Member Price Quantity
Download PDF
$63.00
$84.00