ANSI/AWS D8.8M:1997 SPECIFICATION FOR AUTOMOTIVE AND LIGHT TRUCK COMPONENTS WELD QUALITY ARC WELDING (HISTORICAL)
Member Price: $42.00
Non-Member Price: $56.00
Defined in this specification are practical tolerances needed to achieve satisfactory weld quality when dealing with the production volumes associated with automotive structural parts. Gaps in the weld joints have a significant effect on structural performance and weld quality. Automatic and robotic arc welding requires specified part fit-up in the weld joints for consistent weld quality. Therefore, metal stampings and press-formed parts must be made to produce weld joint fits within the allowable gap of this specification. ANSI Approved. ISBN 0-87171-454-X Historical See AWS D8.8M:2007