Picture of C2.2:1967 RECOMMENDED PRACTICES FOR METALLIZING WITH ALUMINUM AND ZINC FOR PROTECTION OF IRON AND STEEL (HISTORICAL)

C2.2:1967 RECOMMENDED PRACTICES FOR METALLIZING WITH ALUMINUM AND ZINC FOR PROTECTION OF IRON AND STEEL (HISTORICAL)



Member Price: $80.00

Non-Member Price: $80.00

It is intended to present herein a description of the procedures employed in metallizing surfaces with zinc and aluminum where these metals are suitable to protect iron and steel against corrosion. The procedures represent various practices and methods currently used.