A standard 25 Ã? 12 Ã? 80 mm test specimen and method of preparation are set forth, along with two standard methods of diffusible hydrogen analysis, mercury displacement and gas chromatography. The methods are suitable for shielded metal arc welding, gas metal arc welding, flux cored arc welding, and submerged arc welding using welding conditions and electrodes given in several applicable American Welding Society filler metal specifications. ISBN 0-87171-401-9