All Publications

Display per page
  • C2.25/C2.25M:R2018 SPECIFICATION FOR THERMAL SPRAY FEEDSTOCK-WIRE AND RODS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $66.00 Non-Member Price: $88.00

    This specification provides the as-manufactured chemical composition classification requirements for solid and composite wires and ceramic rods for thermal spraying. Requirements f...

    Read More

     
  • A2.4:2012 STANDARD SYMBOLS FOR WELDING, BRAZING, AND NONDESTRUCTIVE EXAMINATION

    Member Price: $153.00 Non-Member Price: $204.00

    Establishes a method of specifying certain welding, brazing, and nondestructive examination information by means of symbols.

    Contains detailed information and exampl...

    Read More

     
  • A5.22/A5.22M:2012 SPECIFICATION FOR STAINLESS STEEL FLUX CORED AND METAL CORED WELDING ELECTRODES AND RODS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $69.00 Non-Member Price: $92.00

    Classification and other requirements are specified for numerous grades of flux cored and metal cored stainless steel electrodes and rods. New classifications include a duplex allo...

    Read More

     
  • G2.5/G2.5M:2012 GUIDE FOR THE FUSION WELDING OF ZIRCONIUM AND ZIRCONIUM ALLOYS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $66.00 Non-Member Price: $88.00

    The standard Guide for the Fusion Welding of Zirconium and Zirconium Alloys provides instructional guidance for the welding of zirconium and zirconium alloys. ISBN: 978-0-87171-802...

    Read More

     
  • A2.1-WC XL:2012 WELDING SYMBOL CHART X-LARGE WALL SIZE

    Member Price: $48.00 Non-Member Price: $64.00

    A wall size (27" X 36") companion to AWS A2.4 2012 Standard Symbols for Welding, Brazing, and Nondestructive Examination, these easy to read wall chart vividly illustrate proper us...

    Read More

     
  • D14.6/D14.6M:2012 SPECIFICATION FOR WELDING OF ROTATING ELEMENTS OF EQUIPMENT (HISTORICAL)

    Member Price: $81.00 Non-Member Price: $108.00

    This specification applies to the fabrication, by welding, of wrought or cast material used to manufacture rotating elements of equipment such as fans, pumps, compressors, and cent...

    Read More

     
  • B2.4:2012 SPECIFICATION FOR WELDING PROCEDURE AND PERFORMANCE QUALIFICATION FOR THERMOPLASTICS (HISTORICAL)

    Member Price: $66.00 Non-Member Price: $88.00

    Defines qualification requirements for welding of thermoplastics. Includes requirements for qualification of Welding Procedure Specifications, welders, and welding operators for ma...

    Read More

     
  • A5.9/A5.9M:2012 SPECIFICATION FOR BARE STAINLESS STEEL WELDING ELECTRODES AND RODS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $69.00 Non-Member Price: $92.00

    This specification prescribes the requirements for classification of solid and composite stainless steel electrodes (both as wire and strip) for gas metal arc welding, submerged ar...

    Read More

     
  • D8.9M:2012 TEST METHODS FOR EVALUATING THE RESISTANCE SPOT WELDING BEHAVIOR OF AUTOMOTIVE SHEET STEEL MATERIALS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $96.00 Non-Member Price: $128.00

    This document presents standard test methods for evaluating the resistance spot welding behavior of automotive sheet steels. The document contains a number of tests and test method...

    Read More

     
  • B2.1-8-216:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX, ER3XX (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with c...

    Read More

     
  • B2.1-8-215:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX AND ER3XX, AS-WELDED CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with c...

    Read More

     
  • B2.1-8-214:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding follow...

    Read More

     
  • B2.1-8-213:1997(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, E3XX-XX, AS-WELDED CONDITION, PRIMARILY PIPE APPLICATIONS (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It ...

    Read More

     
  • B2.1-8-212:2001R(2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR; GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tungsten arc welding. It c...

    Read More

     
  • B2.1-1-211:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METALARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUG1-1/2 INCH THICK, INMS-1, ER70S-2 (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse...

    Read More

     
  • B2.1-1-210:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERTS OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, INMS-1 AND ER70S-2, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse...

    Read More

     
  • B2.1-8-025:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding follow...

    Read More

     
  • B2.1-8-024:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION, PRIMARILY PLATE AND STRUCTURAL APPLICATIONS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tungsten arc welding. It c...

    Read More

     
  • Z49.1:2012 SAFETY IN WELDING AND CUTTING AND ALLIED PROCESSES (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    This standard covers all aspects of safety and health in the welding environment, emphasizing oxygen gas and arc welding processes with some coverage given to resistance welding...

    Read More

     
  • C1.1M/C1.1:2012 RECOMMENDED PRACTICES FOR RESISTANCE WELDING (HISTORICAL)

    Member Price: $96.00 Non-Member Price: $128.00

    This Recommended Practice is a collection of data and procedures that are intended to assist the user in setting up resistance welding equipment to produce resistance welded produc...

    Read More

     
  • A5.31M/A5.31:2012 SPECIFICATION FOR FLUXES FOR BRAZING AND BRAZE WELDING (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    Eighteen fluxes for brazing and braze welding are classified according to the filler metal, form, and activity temperature range. Classification is in accordance with a classificat...

    Read More

     
  • C4.5M:2012 UNIFORM DESIGNATION SYSTEM FOR OXYFUEL NOZZLES

    Formats: Printed Hard Copy, Download PDF

    Member Price: $57.00 Non-Member Price: $76.00

    This document presents recommendations to oxyfuel welding, cutting, and heating/brazing torch nozzle manufacturers regarding the identification markings to be permanently applied t...

    Read More

     
  • D14.4/D14.4M:2012 SPECIFICATION FOR THE DESIGN OF WELDED JOINTS IN MACHINERY AND EQUIPMENT (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $96.00 Non-Member Price: $128.00

    This specification establishes common acceptance criteria for classifying and applying carbon and low-alloy steel welded joints used in the manufacture of machines and equipment. <...

    Read More

     
  • D15.1/D15.1M:2012 AMD1 RAILROAD WELDING SPECIFICATION FOR CARS AND LOCOMOTIVES

    Formats: Printed Hard Copy, Download PDF

    Member Price: $138.00 Non-Member Price: $184.00

    This specification establishes minimum standards for the manufacture and maintenance of railroad equipment. Clauses 4 through 17 cover the general requirements for welding in the r...

    Read More

     
  • D9.1M/D9.1:2012 (HISTORICAL) SHEET METAL WELDING CODE (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $75.00 Non-Member Price: $100.00

    Covers arc and braze welding requirements for nonstructural sheet metal fabrications using commonly welded metals available in sheet form up to and including 3 gauge, or 6.07 mm (0...

    Read More

     
  • A5.1/A5.1M:2012 SPECIFICATION FOR CARBON STEEL ELECTRODES (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $69.00 Non-Member Price: $92.00

    This specification establishes the requirements for classification of carbon steel electrodes for shielded metal arc welding. The requirements include mechanical properties of weld...

    Read More

     
  • B2.3/B2.3M:2012 SPECIFICATION FOR SOLDERING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $75.00 Non-Member Price: $100.00

    This specification provides the requirements for qualification of soldering procedure specifications, solderers, and soldering operators for manual, mechanized, and automatic solde...

    Read More

     
  • D3.6M:2010 (ERRATA 2012) UNDERWATER WELDING CODE (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $102.00 Non-Member Price: $136.00

    This Code covers the requirements for underwater welding of structures and components. It includes welding in both dry and wet environments. Clauses 1 through 6 constitute the gene...

    Read More

     
  • G2.3M/G2.3:2012 GUIDE FOR JOINING OF WROUGHT SOLID SOLUTION AUSTENITIC STAINLESS STEELS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $90.00 Non-Member Price: $120.00

    This guide presents a description of wrought solid solution austenitic stainless steels and the processes and procedures that can be used for the joining of these materials.
    ...

    Read More

     
  • G2.1M/G2.1:2012 GUIDE FOR THE JOINING OF WROUGHT NICKEL-BASED ALLOYS

    Formats: Printed Hard Copy, Download PDF

    Member Price: $72.00 Non-Member Price: $96.00

    The definitive guide to welding metals and alloys not covered by other standards. Learn the guidelines for welding different wrought nickel based alloys, including solidsolution an...

    Read More

     
  • A5.4/A5.4M:2012 SPECIFICATION FOR STAINLESS STEEL ELECTRODES FOR SHIELDED METAL ARC WELDING (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    Composition and other requirements are specified for more than forty classifications of covered stainless steel welding electrodes. The requirements include general requirements, t...

    Read More

     
  • C2.25/C2.25M:2012 SPECIFICATION FOR THERMAL SPRAY FEEDSTOCK-WIRE AND RODS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $66.00 Non-Member Price: $88.00

    This specification classifies solid and composite wires and ceramic rods for thermal spraying, based on their as manufactured chemical composition. Includes requirements for standa...

    Read More

     
  • A2.4:2012 SIMBOLOS ESTANDAR PARA LA SOLDADURA, LA SOLDADURA FUERTE Y LOS ENSAYOS NO DESTRUCTIVOS (SPANISH)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $72.00 Non-Member Price: $72.00

    Esta norma establece un método para especificar, mediante símbolos, cierta información de soldadura, soldadura fuerte y ensayos no destructivos. Se sumi...

    Read More

     
  • Z49.1:2012 SEGURIDAD DE LOS PROCESOS DE SOLDADURA, CORTE Y AFINES (SPANISH)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $36.00 Non-Member Price: $36.00

    Esta norma incluye todos los aspectos de la seguridad y la salud en el ambiente de soldadura, y hace hincapié en los procesos de soldadura con oxígeno y...

    Read More

     
  • ISO 10241-2:2012(E)

    Member Price: $227.00 Non-Member Price: $227.00

    Terminological entries in standards — Part 2: Adoption of standardized terminological entries

    Read More

     
  • A4.5M/A4.5:2012 (ISO 15792-3:2011 MOD) STANDARD METHODS FOR CLASSIFICATION TESTING OF POSITIONAL CAPACITY AND ROOT PENETRATION OF WELDING CONSUMABLES IN A FILLET WELD

    Formats: Printed Hard Copy, Download PDF

    Member Price: $96.00 Non-Member Price: $96.00

    This standard describes preparation and assessment of a fillet weld test piece.

    Test conditions prescribed and results required should not be considered to be requireme...

    Read More

     
  • A5.10/A5.10M:2012 (ISO 18273) WELDING CONSUMABLES–WIRE ELECTRODES, WIRES AND RODS FOR WELDING OF ALUMINUM AND ALUMINUM-ALLOYS–CLASSIFICATION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $69.00 Non-Member Price: $92.00

    This specification prescribes requirements for the classification of bare, wrought and cast aluminum-alloy electrodes and rods for use with the gas metal arc, gas tungsten arc, oxy...

    Read More

     
  • C4.6M:2006(R2012)(ISO 9013:2002 IDT) THERMAL CUTTING-CLASSIFICATION OF THERMAL CUTS-GEOMETRIC PRODUCT SPECIFICATION AND QUALITY TOLERANCES

    Formats: Printed Hard Copy, Download PDF

    Member Price: $261.00 Non-Member Price: $261.00

    This is the U.S. national adoption of ISO 9013:2002, Thermal cutting - Classification of thermal cuts - Geometric product specification and quality tolerances.

    It inclu...

    Read More

     
  • B2.1-1-027:2011 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1/2 INCH THICK, E71T-11, AS-WELDED CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1/2 inch, using semiautomatic, self-shielded flux cored arc welding. I...

    Read More

     
  • C3.11M/C3.11:2011 SPECIFICATION FOR TORCH SOLDERING (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $60.00 Non-Member Price: $80.00

    This specification presents the minimum process and quality requirements for the torch soldering of ceramics, precious metals, and refractory metals, as well as the alloys of coppe...

    Read More

     
  • C3.8M/C3.8:2011 SPECIFICATION FOR THE ULTRASONIC PULSE-ECHO EXAMINATION OF BRAZED JOINTS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $60.00 Non-Member Price: $80.00

    This specification establishes the minimum equipment and procedure requirements for the pulse-echo ultrasonic examination of brazed joints. Its purpose is to standardize brazed-joi...

    Read More

     
  • QC20:2011 SPECIFICATION FOR AWS CERTIFICATION OF RESISTANCE WELDING TECHNICIANS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $21.00 Non-Member Price: $28.00

    This specification defines the certification program of the American Welding Society for use in the Certification of Resistance Welding Technicians (CRWTs). These certifications re...

    Read More

     
  • B5.5:2011 SPECIFICATION FOR THE QUALIFICATION OF WELDING EDUCATORS

    Formats: Printed Hard Copy, Download PDF

    Member Price: $60.00 Non-Member Price: $80.00

    This specification defines the requirements and program to qualify Welding Educators. The qualification of a Welding Educator is determined by a combination of education and experi...

    Read More

     
  • C3.7M/C3.7-2011 SPECIFICATION FOR ALUMINUM BRAZING (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $60.00 Non-Member Price: $80.00

    Addresses the minimum fabrication, equipment, material, process procedure requirements, and inspection requirements for aluminum brazing using the atmosphere furnace, vacuum furnac...

    Read More

     
  • A5.14/A5.14M:2011 SPECIFICATION FOR NICKEL AND NICKEL-ALLOY BARE WELDING ELECTRODES AND RODS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $69.00 Non-Member Price: $92.00

    Covers the chemical compositions of 50 nickel and nickel-alloy welding electrodes and rods are specified, including three compositions not previously classified. Major topics inclu...

    Read More

     
  • A5.23/A5.23M:2011 SPECIFICATION FOR LOW-ALLOY STEEL ELECTRODES AND FLUXES FOR SUBMERGED ARC WELDING (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    This specification provides requirements for the classification of solid and composite carbon steel and low-alloy steel electrodes and fluxes for submerged arc welding. Electrode c...

    Read More

     
  • A5.8M/A5.8:2011 AMD1 SPECIFICATION FOR FILLER METALS FOR BRAZING AND BRAZE WELDING

    Member Price: $69.00 Non-Member Price: $92.00

    This specification prescribes the requirements for the classification of filler metals for brazing and braze welding. The chemical composition, physical form, and packaging of more...

    Read More

     
  • EWH-ALL EFFECTS OF WELDING ON HEALTH VOL 1 THROUGH 14 PLUS INDEX

    Member Price: $174.00 Non-Member Price: $232.00

    Reviews of worldwide medical literature on potential health effects of welding-related physical and chemical hazards. Each volume summarizes studies of occupational exposures, info...

    Read More