All Publications
-
B5.5:2000 SPECIFICATION FOR THE QUALIFICATION OF WELDING EDUCATORS (HISTORICAL)
Member Price: $54.00 Non-Member Price: $72.00
This specification defines the requirements and program to qualify Welding Educators. The qualification of a Welding Educator is determined by a combination of education and exp...
-
D10.12M/D10.12:2000 GUIDE FOR WELDING MILD STEEL PIPE
Formats: Printed Hard Copy, Download PDF
Member Price: $63.00 Non-Member Price: $84.00
The mild steel in this AWS standard refers to lowcarbon less than 0.25 carbon steels such as ASTM A 53, A 106, A 135, A 179, A 524, A 587, and API5L, Grades A25, A and B, and X42. ... -
D10.6/D10.6M:2000 RECOMMENDED PRACTICES FOR GAS TUNGSTEN ARC WELDING OF TITANIUM PIPING AND TUBING
Formats: Printed Hard Copy, Download PDF
Member Price: $60.00 Non-Member Price: $80.00
Incorporates results of research on the effects of atmospheric exposure during welding. Recommended maximum exposure temperature has been lowered and the effects of high temperatur... -
D10.7M/D10.7:2000 GUIDE FOR GAS SHIELDED ARC WELDING OF ALUMINUM AND ALUMINUM ALLOY PIPE (HISTORICAL)
Member Price: $57.00 Non-Member Price: $76.00
Expanded from a Recommended Practice to a Guide, this important pipe welding standard reflects the present state of the art. Sections include welding characteristics of aluminum pr... -
D3.5:1993(R2000) GUIDE FOR STEEL HULL WELDING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $93.00 Non-Member Price: $124.00
This guide provides information to users in the marine construction industry as to the best practical methods to weld steel hulls for ships, barges, mobile offshore drilling units,... -
D8.14M/D8.14:2000 SPECIFICATION FOR AUTOMOTIVE AND LIGHT TRUCK COMPONENTS WELD QUALITY ALUMINUM ARC WELDING (HISTORICAL)
Member Price: $54.00 Non-Member Price: $72.00
Small suppliers will find this manufacturing standard for aluminum automotive components especially helpful. It covers the minimum standards for arc welding of aluminum components ... -
FMC:2000 FILLER METAL COMPARISON CHARTS
Member Price: $168.00 Non-Member Price: $224.00
More than 80 producers and marketers of filler metals have supplied trade names of thousands of products conforming to AWS filler metal classifications.
Products are ta... -
D1.1:2000 STRUCTURAL WELDING CODE - STEEL (HISTORICAL)
Member Price: $333.00 Non-Member Price: $444.00
STRUCTURAL WELDING CODE STEEL, REV. 2000 HISTORICAL COPY -
C4.5M:2000 UNIFORM DESIGNATION SYSTEM FOR OXYFUEL NOZZLES (HISTORICAL)
Member Price: $51.00 Non-Member Price: $68.00
This document presents recommendations to oxyfuel welding, cutting, and heating/brazing torch nozzle manufacturers regarding the identification markings to be permanently applied t... -
D9.1M/D9.1:2000 SHEET METAL WELDING CODE (HISTORICAL)
Member Price: $69.00 Non-Member Price: $92.00
This code covers the arc and braze welding requirements for nonstructural sheet metal fabrications using the commonly welded metals available in sheet form. Requirements and limita... -
CM CERTIFICATION MANUAL FOR WELDING INSPECTORS (AWS CM)
Formats: Printed Hard Copy, Download PDF
Member Price: $177.00 Non-Member Price: $236.00
Self-study to prepare for AWS welding inspector exams. An excellent reference and introduction for those studying for the CWI examination. An updated version of the bestseller used... -
WI:2000 WELDING INSPECTION HANDBOOK
Member Price: $75.00 Non-Member Price: $100.00
This invaluable raining refernce helps inspectors, engineers, and welders evaluate the difference be...
-
WIT-T:2000 WELDING INSPECTION TECHNOLOGY (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $258.00 Non-Member Price: $344.00
For at home study, you can purchase this official reference textbook for the three day AWS core seminar for CWI exam preparation. You'll find this newest Welding Inspection Technol... -
WIT-T:2000 WELDING INSPECTION TECHNOLOGY (SPANISH)
Formats: Printed Hard Copy, Download PDF
Member Price: $116.00 Non-Member Price: $116.00
For at home study, you can purchase this official reference textbook for the three day AWS core seminar for CWI exam preparation. You'll find this newest Welding Inspection Technol... -
A5.3/A5.3M:1999(R2007) SPECIFICATION FOR ALUMINUM AND ALUMINUM ALLOY ELECTRODES FOR SHIELDED METAL ARC WELDING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes requirements for the classification of covered (flux coated) E1100,E3003, and E4043 aluminium-alloy electrodes for shielded metal arc welding. Test...
-
AWS ARC WELDING AND CUTTING SAFETY SET OF 25 PAMPHLETS
Member Price: $36.00 Non-Member Price: $48.00
As in most trades, welders are exposed to certain hazards. Hazards exist with all arc welding and allied processes. Welding is safe when safe practices are followed. This booklet i... -
B1.10:1999 GUIDE FOR THE NONDESTRUCTIVE EXAMINATION OF WELDS (HISTORICAL)
Member Price: $99.00 Non-Member Price: $132.00
This guide acquaints the user with the nondestructive examination methods commonly used the examine weldments. The standard also addresses which method best detects various types o... -
B2.1-5A-224:1999 STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL, (M-5A/P-5A), 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 INCH THICK, PWHT (HISTORICAL)
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 through 1-1/2 ... -
B2.1-5A-225:1999 STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW (CONSUMABLE INSERT ROOT) OF CHROMIUM-MOLYBDENUM STEEL, (M-5A/P-5A), 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 3/4 INCH THICK, PWHT CONDITION, IN521 (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 through 3/4 in... -
B2.1-5A-226:1999 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING (CONSUMABLE INSERT ROOT) FOLLOWED BY SHIELDED METAL ARCWELDING OF CHROMIUM-MOLYBDENUM STEEL, (M-5A/P-5A), 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 through 1-1/2 ... -
C1.4M/C1.4:1999 SPECIFICATION FOR RESISTANCE WELDING OF CARBON AND LOW-ALLOY STEELS (HISTORICAL)
Member Price: $54.00 Non-Member Price: $72.00
This specification establishes welding equipment and procedure requirements, material preparation, and preproduction requirements for acceptable welds in coated and uncoated, lowca... -
D1.6:1999 STRUCTURAL WELDING CODE STAINLESS STEEL (HISTORICAL)
Member Price: $129.00 Non-Member Price: $172.00
This code establishes the requirements for welding stainless steel using the gas metal, shielded metal, flux cored, and submerged arc welding processes, including stud welding. The... -
D10.10/D10.10M:1999 RECOMMENDED PRACTICES FOR LOCAL HEATING OF WELDS IN PIPING AND TUBING (HISTORICAL)
Member Price: $84.00 Non-Member Price: $112.00
The current revision of this popular standard considers both local 360 band and spot heating thermocouple location, attachment and accuracy insulation provisions service environmen... -
D18.1: 1999 SPECIFICATION FOR WELDING OF AUSTENITIC STAINLESS STEEL TUBE AND PIPE SYSTEMS IN SANITARY (HYGIENIC) APPLICATIONS (HISTORICAL)
Member Price: $57.00 Non-Member Price: $76.00
This document outlines welding standards for use in the manufacture and construction of dairy and food product processing plants. Compiled at the request of the 3A Sanitary Standar... -
D3.6M:1999 SPECIFICATION FOR UNDERWATER WELDING (HISTORICAL)
Member Price: $96.00 Non-Member Price: $128.00
This specification covers the requirements for underwater welding of structures and components. It includes welding in both dry and wet environments. Sections 1 through 6 constitut... -
DPW:1999 DESIGN AND PLANNING MANUAL FOR COST EFFECTIVE WELDING (DPW)
Formats: Printed Hard Copy, Download PDF
Member Price: $102.00 Non-Member Price: $136.00
A practical guide for engineers, planners, and handson professionals to improve scheduling and lessen rework regardless of industry. Past AWS board member Eugene Hornberger has edi... -
EWH-12 EFFECTS OF WELDING ON HEALTH
Formats: Printed Hard Copy, Download PDF
Member Price: $51.00 Non-Member Price: $68.00
Reviews of the worldwide medical literature on potential health effects of welding related physical and chemical hazards. Each volume in the series summarizes recent studies of occ... -
F4.1:1999 RECOMMENDED SAFE PRACTICES FOR THE PREPARATION FOR WELDING AND CUTTING OF CONTAINERS AND PIPING (HISTORICAL)
Member Price: $51.00 Non-Member Price: $68.00
This standard informs the reader of necessary safe practices for cleaning and preparing to weld and cut containers and piping. It describes various cleaning methods including wate... -
SHB:1999 SOLDERING HANDBOOK, SOFTBOUND, 3RD ED
Formats: Printed Hard Copy, Download PDF
Member Price: $144.00 Non-Member Price: $192.00
Contains information related to soldering processes, and solder joint performance and reliability. Covers soldering fundamentals, technology, materials, substrate materials, fluxes... -
B2.1-4-217:1999 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CHROMIUM - MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 or 2), ER80S-B2, 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 3/4 INCH THICK (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 through 3/4 in... -
B2.1-4-218:1999 STANDARD WELDING PROCEDURE SPECIFICATION FOR SMAW OF CHROMIUM - MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 or 2), E8018-B2, 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 INCH THICK, PWHT CONDITION (HISTORICAL)
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 in. through 1-... -
A5.9:1993(R1999) SPECIFICATION FOR BARE STAINLESS STEEL WELDING ELECTRODES AND RODS (HISTORICAL)
Member Price: $69.00 Non-Member Price: $92.00
The classification and other requirements for more than forty-five bare stainless steel electrodes (solid and composite), rods, and strips are specified, including a number of dupl... -
F1.1:1999 METHOD FOR SAMPLING AIRBORNE PARTICULATES GENERATED BY WELDING AND ALLIED PROCESSES (HISTORICAL)
Member Price: $54.00 Non-Member Price: $72.00
This document aids the reader in the proper technique for sampling welding fume in the workplace. Emphasis is placed on positioning the sampling device and calibration of the equip... -
F1.3M:1999 A SAMPLING STRATEGY GUIDE FOR EVALUATING CONTAMINANTS IN THE WELDING ENVIRONMENT (HISTORICAL)
Member Price: $57.00 Non-Member Price: $76.00
This guide provides advice on contaminants that may be present in the welding environment, and presents a strategy for collecting valid samples from the welder’s breathing zone. Re... -
B1.10:1999 GUIA PARA EL ENSAYO NO DESTRUCTIVO DE SOLDADURAS (SPANISH) (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $52.00 Non-Member Price: $52.00
Esta guía familiariza al usuario con los métodos de ensayo...
-
SHC1 SOLDERING HANDBOOK CHAPTER 1: FUNDAMENTALS OF SOLDERING TECHNOLOGY
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 1: FUNDAMENTALS OF SOLDERING TECHNOLOGY
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can fi... -
SHC2 SOLDERING HANDBOOK CHAPTER 2: SOLDER MATERIALS
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 2: SOLDER MATERIALS
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find it hereRead More -
SHC3 SOLDERING HANDBOOK CHAPTER 3: SUBSTRATE MATERIALS
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 3: SUBSTRATE MATERIALS
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find it here
<... -
SHC4 SOLDERING HANDBOOK CHAPTER 4: FLUXES
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 4: FLUXES
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find it hereRead More -
SHC5 SOLDERING HANDBOOK CHAPTER 5: SOLDER PASTES
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 5: SOLDER PASTES
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find it here
Read More -
SHC6 SOLDERING HANDBOOK CHAPTER 6: ASSEMBLY PROCESSES
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 6: ASSEMBLY PROCESSES
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find it here
... -
SHC7 SOLDERING HANDBOOK CHAPTER 7: INSPECTION TECHNIQUES FOR PRODUCE ACCEPTANCE AND PROCESS OPTIMIZATION
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 7: INSPECTION TECHNIQUES FOR PRODUCE ACCEPTANCE AND PROCESS OPTIMIZATION
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy... -
SHC8 SOLDERING HANDBOOK CHAPTER 8: ENVIRONMENTAL, SAFETY AND HEALTH
Member Price: $27.00 Non-Member Price: $36.00
SOLDERING HANDBOOK CHAPTER 8: ENVIRONMENTAL, SAFETY AND HEALTH
DIGITAL PDF FORMAT ONLY
If you want the entire hardcopy with all the chapters you can find i... -
B2.1-1-027:1998 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2),1/8 THROUGH 1/2 INCH THICK, E71T-11, AS-WELDED CONDITION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1/2 inch, using semiautomatic, self-shielded flux cored arc welding. I... -
B4.0:1998 STANDARD METHODS FOR MECHANICAL TESTING OF WELDS (US CUSTOMARY UNITS) (HISTORICAL)
Member Price: $75.00 Non-Member Price: $100.00
Describes the most common mechanical test methods applicable to welds and welded joints. Each test method gives details concerning specimen preparation, test parameters, testing pr... -
C7.2:1998 RECOMMENDED PRACTICES FOR LASER BEAM WELDING, CUTTING, AND DRILLING (HISTORICAL)
Member Price: $84.00 Non-Member Price: $112.00
This document presents recommended practices for laser beam welding, cutting, and drilling. It is intended to cover common applications of the process. Processes definitions, safe ... -
D1.1 BI THE OFFICIAL BOOK OF D1.1 INTERPRETATIONS; A COLLECTION OF RESPONSES TO FORMAL INQUIRIES ABOUT THE REQUIREMENTS OF AWS D1.1 (1976-1998) (HISTORICAL)
Member Price: $69.00 Non-Member Price: $92.00
A collection of responses to formal inquiries about the requirements of AWS D1.1 from 1976 to 1998. An excellent reference for AWS D1.1 users. (Historical) AVAILABLE IN PHOTOCOPY O... -
D10.4:1986R PRINTING RECOMMENDED PRACTICES FOR WELDING AUSTENITIC CHROMIUM NICKEL STAINLESS STEEL PIPING AND TUBING (HISTORICAL)
Member Price: $66.00 Non-Member Price: $88.00
This document presents a detailed discussion of the metallurgical characteristics and weldability of many grades of austenitic stainless steel used in piping and tubing. The delta ...
Cart