  • D15.1:1986 RAILROAD WELDING SPECIFICATION CARS AND LOCOMOTIVES (HISTORICAL)

    Member Price: $213.00 Non-Member Price: $284.00

    This specification establishes minimum standards for the manufacture and maintenance of railroad equipment. Sections A through E (Part I) cover the general requirements for welding...

    Read More

     
  • TPW - THE PHYSICS OF WELDING SECOND EDITION

    Member Price: $92.00 Non-Member Price: $92.00

    The Physics of Welding, Second Edition covers topics in welding physics. The book describes symbols, units and dimensions; the physical prop...

    Read More

     
  • EWH-6 EFFECTS OF WELDING ON HEALTH

    Formats: Printed Hard Copy, Download PDF

    Member Price: $51.00 Non-Member Price: $68.00

    This literature review with 172 citations has been prepared for the Safety and Health Committee of the American Welding Society to provide an assessment of current knowledge of the...

    Read More

     
  • TSS:1985 THERMAL SPRAYING; PRACTICE THEORY, AND APPLICATION (HISTORICAL)

    Member Price: $84.00 Non-Member Price: $112.00

    The thermal spraying processes are specialized, yet have a wide ranging utilization in both manufacturing and maintenance. The nature of the processes is truly synergistic. That is...

    Read More

     
  • D14.1-1985 SPECIFICATION FOR WELDING OF INDUSTRIAL AND MILL CRANES AND OTHER MATERIAL HANDLING EQUIPMENT (PHOTO COPY ONLY)

    Member Price: $138.00 Non-Member Price: $184.00

    Overhead cranes and material handling equipment that utilize plate girders and other welded plate structures rather than the rolled beams normally used in fabricating steel for bri...

    Read More

     
  • A5.6:1984 COVERED COPPER AND COPPER ALLOY ARC WELDING ELECTRODES (HISTORICAL)

    Member Price: $54.00 Non-Member Price: $72.00

    This specification provides requirements for the classification of covered copper and copper alloy electrodes for shielded metal arc welding. It includes compositions in which the ...

    Read More

     
  • EWH-5 EFFECTS OF WELDING ON HEALTH

    Formats: Printed Hard Copy, Download PDF

    Member Price: $51.00 Non-Member Price: $68.00

    This literature review with 105 citations has been prepared for the Safety and Health Committee of the American Welding Society to provide an assessment of current knowledge of the...

    Read More

     
  • CAWF CHARACTERIZATION OF ARC WELDING FUMES

    Formats: Printed Hard Copy, Download PDF

    Member Price: $72.00 Non-Member Price: $96.00

    Six welding fumes, representing a variety of welding rods and wires, were analyzed for particle size and chemistry by X-ray diffraction, energy dispersive X-ray analysis, scanning ...

    Read More

     
  • D3.6M:1983 SPECIFICATION FOR UNDERWATER WELDING (HISTORICAL)

    Member Price: $63.00 Non-Member Price: $84.00

    This specification contains four underwater weld t...

    Read More

     
  • EWH-4 EFFECTS OF WELDING ON HEALTH

    Formats: Printed Hard Copy, Download PDF

    Member Price: $51.00 Non-Member Price: $68.00

    This literature review has been prepared for the Safety and Health Committee of the American Welding Society to provide an assessment of current knowledge of the effects of welding...

    Read More