AWS-NAVSEA B2.1-8-309:2018 - Standard Welding Procedure Specification for Naval Applications for Shielded Metal Arc Welding of Austenitic Stainless Steel, 1/8 " [3 mm] through 1-1/2" [38 mm] Thick, MIL-3XX-XX, in the As-Welded Condition
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded...
-
AWS-NAVSEA B2.1-8-319:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Shielded Metal Arc Welding of Austenitic Stainless Steel (S-8), 1/8"[3 mm] through 1-1/2"[38 mm] Thick, MIL-3XX-XX, in the As-Welded Cond., Primarily Pipe for Naval Apps
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded...
-
AWS-NAVSEA B2.1-1-311:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Gas Tungsten Arc Welding of Carbon Steel (S-1), 1/8"[3 mm] through 1-1/2"[38 mm] Thick, MIL-70S-2, in the As-Welded or PWHT Condition, Primarily Pipe for Naval Apps.
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc weldi...
-
AWS-NAVSEA B2.1-1-304:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for CO2 Shielded Flux Cored Arc Welding of Carbon Steel (S-1), 1/8" [3mm] through 1-1/2" [38mm] Thick, MIL-70T-1, MIL-71T-1, As-Welded Cond., Plate and Struc. Naval Apps.
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic carbon dioxide shi... -
AWS-NAVSEA B2.1-1-305:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for 75% Argon Plus 25% Carbon Dioxide Shielded Flux Cored Arc Welding of Carbon Steel (S-1), MIL-70T-1 and MIL-71T-1
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic gas shielded flux ... -
AWS-NAVSEA B2.1-1-316:2018-Standard Welding Procedure Specification for Naval Applications for Argon Plus 2% Oxygen Shielded Gas Metal Arc Welding (Spray Transfer) of Carbon Steel (S-1), 1/8 in [3 mm] through 1-1/2 in [38 mm] Thick, MIL-70S-3
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic gas metal arc weld... -
AWS-NAVSEA B2.1-1-317:2018 - Standard Welding Procedure Specification for Naval Applications for 75% Ar+25% CO2 Shielded Flux Cored Arc Welding of Carbon Steel (S-1), 1/8"[3 mm] --> 1-1/2"[38 mm] Thick, MIL-70T-1, MIL-71T-1, in As-Welded or PWHT Cond., Primarily Pipe for Naval Apps.
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic gas shielded fl...
-
AWS B2.1-1-027:2018 (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1/2 inch [13 mm], using self-shielded flux cored arc we...
-
A5.2/A5.2M:2018 SPECIFICATION FOR CARBON AND LOW-ALLOY STEEL RODS FOR OXYFUEL GAS WELDING (HISTORICAL)
Member Price: $69.00 Non-Member Price: $92.00
Read More -
B2.3/B2.3M:2018 SPECIFICATION FOR SOLDERING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $84.00 Non-Member Price: $112.00
This specification provides the requirements for qualifica...