D1.2/D1.2M:2014 STRUCTURAL WELDING CODE -ALUMINUM (HISTORICAL)
Member Price: $198.00
Non-Member Price: $264.00
This code covers the welding requirements for any type structure made from aluminum structural alloys, except for aluminum pressure vessels and pressure piping. Clauses 1 through 8 constitute a body of rules for the regulation of welding in aluminum construction. A commentary on the code is also included with the document. ISBN: 978-0-87171-840-2