The chemical compositions of nearly fifty nickel and nickel-alloy welding electrodes and rods are specified, including thirteen compositions not previously classified. Major topics include general requirements, testing, packaging and application guidelines. This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other. ISBN 0-87171-007-2. See AWS A5.14/A5.14M :2009 for new revision.