Picture of A5.14/A5.14M:2009 SPECIFICATION FOR NICKEL AND NICKEL-ALLOY BARE WELDING ELECTRODES AND RODS (HISTORICAL)

A5.14/A5.14M:2009 SPECIFICATION FOR NICKEL AND NICKEL-ALLOY BARE WELDING ELECTRODES AND RODS (HISTORICAL)

ERRATA FOR THIS CODE PROVIDED, CLICK HERE



Member Price: $69.00

Non-Member Price: $92.00

Covers the chemical compositions of 50 nickel and nickel-alloy welding electrodes and rods are specified, including three compositions not previously classified. Major topics include general requirements, testing, packaging, and application guidelines. This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other.