Picture of B2.1-1-022:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010 (VERTICAL UPHILL) FOLLOWED BY E7018, AS-WELDED OR PWHT CONDITION (HISTORICAL)

B2.1-1-022:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010 (VERTICAL UPHILL) FOLLOWED BY E7018, AS-WELDED OR PWHT CONDITION (HISTORICAL)



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This WPS was developed primarily for plate and structural applications. ISBN 0-87171-431-0

Formats Member Price Non-Member Price Quantity
Download PDF
$264.00
$352.00