D11.2:1989(R2006) GUIDE FOR WELDING IRON CASTINGS (HISTORICAL)
Member Price: $86.00
Non-Member Price: $115.00
This standard presents briefly the history and metallurgy of cast iron and the welding processes applicable to it. A newly developed weld ability test is described in detail and instructions given for its application in specific cases. Provision is made for qualification of welding procedures and welders when necessary; quality control practice is also included. ISBN 0-87171-295-4