AWS-NAVSEA B2.1-8-319:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Shielded Metal Arc Welding of Austenitic Stainless Steel (S-8), 1/8"[3 mm] through 1-1/2"[38 mm] Thick, MIL-3XX-XX, in the As-Welded Cond., Primarily Pipe for Naval Apps
Member Price: $264.00
Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and joint designs for groove and fillet welds. This SWPS-N was developed primarily for naval applications that require performance to NAVSEA Technical Publication S9074-AQ-GIB-010/248, Requirements for Welding and Brazing Procedure and Performance Qualification.ISBN: 978-0-87171-938-6