AWS D17.2/D17.2M-2019 SPECIFICATION FOR RESISTANCE WELDING FOR AEROSPACE APPLICATIONS (HISTORICAL)
Member Price: $75.00
Non-Member Price: $100.00
This specification provides the general resistance welding requirements for aerospace hardware. It includes, but is not limited to, resistance spot and resistance seam welding of aluminum, magnesium, iron, nickel, cobalt, and titanium-based alloys. There are requirements for machine and welding schedule qualification, production witness samples, and inspection and acceptance criteria for aerospace hardware.ISBN Print: 978-0-87171-952-2 ISBN PDF: 978-1-64322-020-8