D15.1/D15.1M:2019 RAILROAD WELDING SPECIFICATION FOR CARS AND LOCOMOTIVES



Member Price: $129.00

Non-Member Price: $172.00

This specification establishes minimum welding standards for the manufacture and maintenance of railcars, locomotives, and their components, intended for North American railroad service. Clauses 4 through 17 cover the general requirements
for welding in the railroad industry. Clauses 18 through 23 cover specific requirements for the welding of base metals thinner than 1/8 in [3 mm]. ISBN Print: 978-1-64322-050-5 ISBN PDF: 978-1-64322-051-2