Picture of D14.4/D14.4M:2019 SPECIFICATION FOR THE DESIGN OF WELDED JOINTS IN MACHINERY AND EQUIPMENT

D14.4/D14.4M:2019 SPECIFICATION FOR THE DESIGN OF WELDED JOINTS IN MACHINERY AND EQUIPMENT



Member Price: $105.00

Non-Member Price: $140.00

This specification establishes common acceptance criteria for classifying and applying carbon and low-alloy steel welded joints used in the manufacture of machines and equipment. It also covers weld joint design, workmanship, quality
control requirements and procedures, weld joint inspection, nondestructive testing, repair of weld defects, and postweld treatment. ISBN Print: 978-1-64322-064-2 ISBN PDF: 978-1-64322-065-9 

D14.0 replaced D14.4