D8.9M:2022 - TEST METHODS FOR EVALUATING THE RESISTANCE SPOT WELDING BEHAVIOR OF AUTOMOTIVE SHEET STEEL MATERIALS



Member Price: $91.00

Non-Member Price: $121.00

This document presents standard test methods for evaluating the resistance spot welding behavior of automotive sheet steels. The document contains a number of tests and test methods useful in determining the resistance spot welding performance
of coated and uncoated automotive sheet steels of all strength levels and compositions. The test methods are designed to assess current range, electrode endurance, and weld properties of automotive sheet steels. The weld property
tests include tests for hold time sensitivity, weld hardness, shear tension strength, and cross tension strength. ISBN Print: 978-1-64322-211-0  ISBN Print: 978-1-64322-212-7