D1.4/D1.4M:2018-AMD1 STRUCTURAL WELDING CODE -STEEL REINFORCING BARS
Member Price: $129.00
Non-Member Price: $172.00
This code covers the requirements for welding steel reinforcing bars in most reinforced concrete applications. It contains a body of rules for the regulations of welding steel reinforcing bars and provides suitable acceptance criteria for such welds.