Picture of D1.4/D1.4M:2005 STRUCTURAL WELDING CODE  REINFORCING STEEL (HISTORICAL)

D1.4/D1.4M:2005 STRUCTURAL WELDING CODE REINFORCING STEEL (HISTORICAL)



Member Price: $90.00

Non-Member Price: $120.00

Covers welding of reinforcing steel in most reinforced concrete applications. Includes sections on allowable stresses, structural details, workmanship requirements, technique, procedure and performance qualification, and inspection. Figures clearly illustrate important welding considerations; unacceptable weld profiles, effective weld sizes, details of joints of anchorages, base plates, and inserts. New in this edition. A comprehensive approach to radiographic testing of reinforcing steel welds, a section on weld cleaning, welder qualifications requirements and testing for fillet welds, and updated forms for welding, testing and inspection. 6th edition. ISBN 0-87171-004-8

Formats Member Price Non-Member Price Quantity
Download PDF
$90.00
$120.00