A5.4/A5.4M:2006 SPECIFICATION FOR STAINLESS STEEL ELECTRODES FOR SHIELDED METAL ARC WELDING (HISTORICAL)
Member Price: $66.00
Non-Member Price: $88.00
Composition and other requirements are specified for more than forty classifications of covered stainless steel welding electrodes. The requirements include general requirements, testing, and packaging. Annex A provides application guidelines and other useful information about the electrodes. This specification makes use of both U.S. Customary Units and the International System of Units {SI}. Since these are not equivalent, each system must be used independently of the other.