A5.4/A5.4M:2012(R2022) SPECIFICATION FOR STAINLESS STEEL ELECTRODES FOR SHIELDED ARC WELDING



Member Price: $66.00

Non-Member Price: $88.00

Composition and other requirements are specified for more than forty classifications of covered stainless steel welding electrodes. The requirements include general requirements, testing, and packaging.

Annex A provides application guidelines and other useful information about the electrodes.

This specification makes use of both U.S. Customary Units and the International System of Units [SI]. Since these are not equivalent, each system must be used independently of the other.