AWS Filler Metal Specifications by Material and Welding Process
| OFW | SMAW | GTAW GMAW PAW | FCAW | SAW | ESW | EGW | BRAZING | THERMAL SPRAYING | |
| Carbon Steel | A5.2 | A5.1 | A5.18 | A5.36 | A5.20 | A5.36 | A5.17 | A5.25 | A5.26 | A5.8 | A5.31 | C2.25 |
| Low-Alloys Steel | A5.2 | A5.5 | A5.28 | A5.36 | A5.29 | A5.36 | A5.23 | A5.25 | A5.26 | A5.8 | A5.31 | C2.25 |
| Stainless Steel | A5.4 | A5.9 | A5.22 | A5.9 | A5.9 | A5.9 | A5.8 | A5.31 | C2.25 | |
| Cast Iron | A5.15 | A5.15 | A5.15 | A5.15 | A5.8 | A5.31 | ||||
| Nickel Alloys | A5.11 | A5.14 | A5.34 | A5.14 | A5.14 | A5.8 | A5.31 | C2.25 | ||
| Aluminum Alloys | A5.3 | A5.10 | A5.8 | A5.31 | C2.25 | |||||
| Copper Alloys | A5.6 | A5.7 | A5.8 | A5.31 | C2.25 | |||||
| Titanium Alloys | A5.16 | A5.8 | A5.31 | |||||||
| Zirconium Alloys | A5.24 | A5.8 | A5.31 | |||||||
| Magnesium Alloys | A5.19 | A5.8 | A5.31 | |||||||
| Tungsten Electrodes | A5.12 | ||||||||
| Brazing Alloys and Fluxes | A5.8 | A5.31 | ||||||||
| Surfacing Alloys | A5.21 | A5.13 | A5.21 | A5.21 | A5.21 | C2.25 | |||
| Consumable Inserts | A5.30 | ||||||||
| Shielding Gases | A5.32 | A5.32 | A5.32 | ||||||
| Ceramics | C2.25 | ||||||||