Carbon Steel
-
B2.1-1-233:2020 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 75% ARGON PLUS 25% CARBON DIOXIDE SHIELDED GAS METAL ARC WELDING (SHORT CIRCUITING TRANSFER MODE) FOLLOWED BY 98% ARGON PLUS 2% OXYGEN
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using 75% argon plus 25% carbon dio...
-
A5.28/A5.28M:2020 SPECIFICATION FOR LOW-ALLOY STEEL ELECTRODES AND RODS FOR GAS SHIELDED ARC WELDING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for classification of solid... -
B2.1-1-234:2020-AMD1 - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 75% ARGON PLUS 25% CARBON DIOXIDE SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL , IN THE AS-WELDED OR PWHT CONDITION, PRIMARILY PIPE APPLICATIONS (2ND PRINTING)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using 75% argon plus 25% carbon dioxid... -
B2.1-1-235:2020-AMD1-STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 98% ARGON PLUS 2% OXYGEN SHIELDED GAS METAL ARC WELDING (SPRAY TRANSFER MODE) OF CARBON STEEL , IN THE AS-WELDED OR PWHT CONDITION, PRIMARILY PIPE APPLICATIONS (2ND PRINTING)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using 98% argon plus 2% oxygen shielde... -
B2.1-1-201:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL (M-1/P-1, GROUP 1 OR 2), 1/8 INCH [3 MM] THROUGH 3/4 INCH [19 MM] THICK, E6010 (VERTICAL UPHILL) FOLLOWED BY E7018 (VERTICAL UPHILL), IN THE AS-WELDED CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 3/4 inch [19 mm], using manual shielded metal arc welding ... -
B2.1-1-203:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 3/4 INCH THICK, E6010 (VERTICAL UPHILL), AS-WELDED CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 3/4 inch [19 mm], using manual shielded metal arc weldi...
-
B2.1-1-204:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 3/4 INCH THICK, E6010 (VERTICAL DOWNHILL ROOT WITH THE BALANCE VERTICAL UPHILL), AS-WELDED CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 3/4 inch [19 mm], using manual shielded metal arc weldi...
-
B2.1-1-205:2019 STANDARD WELDING PROCEDURE SPECIFICATION FOR SMAW OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010 (VERTICAL UPHILL) FOLLOWED BY E7018 (VERTICAL UPHILL), AS-WELDED OR PWHT CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded metal arc wel...
-
B2.1-1-206:2019 STANDARD WELDING PROCEDURE SPECIFICATION FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010 FOLLOWED BY E7018 AS-WELDED OR PWHT CONDITION, PRIMARILY PIPE APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded metal arc wel...
-
B2.1-1-207:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, ER70S-2, AS-WELDED OR PWHT CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc welding....
Cart