All Publications
-
B5.17:2025-AMD1 - SPECIFICATION FOR THE QUALIFICATION OF WELDING FABRICATORS
Member Price: $69.00 Non-Member Price: $92.00
This standard establishes the minimum requirements necessary to qualify as a Welding Fabricator. The qualification is determined based on an examination of the implementation of...
-
B5.16:2025 - SPECIFICATION FOR THE QUALIFICATION OF WELDING ENGINEERS
Member Price: $66.00 Non-Member Price: $88.00
This specification establishes the requirements for qualification of Welding Engineering Technologists and Welding Engineers employed in the welding industry. The minimum experi...
-
A3.1:2025 MASTER CHART OF WELDING AND JOINING PROCESSES
Member Price: $45.00 Non-Member Price: $60.00
AWS Master Chart of Welding and Joining Processes. -
A3.0M/A3.0:2025 STANDARD WELDING TERMS AND DEFINITIONS INCLUDING TERMS FOR ADDITIVE MANUFACTURING, ADHESIVE BONDING, BRAZING,SOLDERING,THERMAL CUTTING, THERMAL SPRAYING, AND NONDESTRUCTIVE EXAMINATION
Formats: Printed Hard Copy, Download PDF
Member Price: $201.00 Non-Member Price: $268.00
This standard is a glossary of the technical terms used in the welding industry. Its purpose is to establish standard terms to aid in the communication of information related to we... -
B5.1:2025 - SPECIFICATION FOR THE QUALIFICATION OF WELDING INSPECTORS
Member Price: $66.00 Non-Member Price: $88.00
This standard defines the qualification requirements to qualify welding inspectors. The qualification requirements for visual welding inspectors include experience and satisfa... -
A5.1/A5.1M:2025 - SPECIFICATION FOR CARBON STEEL ELECTRODES FOR SHIELDED METAL ARC WELDING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for classification of carbon steel covered electrodes used for shielded
metal arc welding. The requirements include chemical ... -
A5.02/A5.02M:2025 - SPECIFICATION FOR FILLER METAL STANDARD SIZES, PACKAGING, AND PHYSICAL ATTRIBUTES
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for standard sizes and packages of welding filler metals, allowing these
physical attributes to be incorporated by reference ... -
B5.4:2025 - SPECIFICATION FOR THE QUALIFICATION OF WELDER TEST FACILITIES
Member Price: $66.00 Non-Member Price: $88.00
This specification defines the requirements for the qualification of welder test facilities.
THIS PUBLICATION IS AVAILABLE FOR FREE AS A DOWNLOAD (PDF). PLEASE <...
-
C2.26/C2.26M:2025 - SPECIFICATION FOR THERMAL SPRAY POWDER
Formats: Printed Hard Copy, Download PDF
Member Price: $81.00 Non-Member Price: $108.00
This specification establishes the requirements for the classification of powders for various thermal spraying processes.
The requirements include particle size distributio... -
D15.1/D15.1M:2025 - RAILROAD WELDING SPECIFICATION FOR CARS AND LOCOMOTIVES
Formats: Printed Hard Copy, Download PDF
Member Price: $165.00 Non-Member Price: $220.00
This specification establishes minimum welding standards for the manufacture and maintenance of railcars, locomotives,
and their components, intended for North American railro... -
C2.27/C2.27M:2025 - GUIDE TO THERMAL SPRAY MASKING
Formats: Printed Hard Copy, Download PDF
Member Price: $75.00 Non-Member Price: $100.00
This guide presents efficient strategies for various thermal spray processes to improve masking effectiveness, minimize
cost, and avoid and address common issues. Workpiece pr... -
(PUBLIC REVIEW) D8.2-E2-DS1 - SPECIFICATION FOR AUTOMOTIVE WELD QUALITY--RESISTANCE SPOT WELDING OF ALUMINUM
Member Price: $44.00 Non-Member Price: $44.00
This document contains both visual and measurable acceptance criteria for resistance spot welds in aluminum. The information contained herein may be used as an aid by designers, re... -
D1.8/D1.8M:2025 - STRUCTURAL WELDING CODE — SEISMIC SUPPLEMENT
Formats: Printed Hard Copy, Download PDF
Member Price: $183.00 Non-Member Price: $244.00
This code supplements the requirements of AWS D1.1/D1.1M, Structural Welding Code—Steel. This code is intended to
be applicable to welded joints in Seismic Force Resisting Sys... -
A5.23/A5.23M:2025 - SPECIFICATION FOR LOW-ALLOY AND HIGH MANGANESE STEEL ELECTRODES AND FLUXES FOR SUBMERGED ARC WELDING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification provides requirements for the classification of solid and composite carbon steel, low-alloy steel, and high manganese steel electrodes and fluxes for submerge...
-
A5.17/A5.17M:2025 - SPECIFICATION FOR CARBON STEEL ELECTRODES AND FLUXES FOR SUBMERGED ARC WELDING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification provides requirements for the classification of solid and composite carbon steel electrodes and fluxes for submerged arc welding. Electrode classification is ...
-
B5.17:2025 - SPECIFICATION FOR THE QUALIFICATION OF WELDING FABRICATORS
Member Price: $69.00 Non-Member Price: $92.00
This standard establishes the minimum requirements necessary to qualify as a Welding Fabricator. The qualification is determined based on an examination of the implementation of th... -
AASHTO/AWS D1.5M/D1.5:2025 - BRIDGE WELDING CODE
Formats: Printed Hard Copy, Download PDF
Member Price: $432.00 Non-Member Price: $576.00
This code covers the welding requirements for welded bridges made from carbon and low-alloy constructional steels and
designed to AASHTO or AREMA requirements. This 2025 ed... -
D16.4M/D16.4:2025 - SPECIFICATION FOR THE QUALIFICATION OF ROBOTIC ARC WELDING PERSONNEL
Formats: Printed Hard Copy, Download PDF
Member Price: $66.00 Non-Member Price: $88.00
This specification provides requirements for the qualification of robotic arc welding personnel at three different
classifications—Associate Technician (AT), Technician (T), a... -
G2.5/G2.5M:2025 - GUIDE FOR THE FUSION WELDING OF ZIRCONIUM AND ZIRCONIUM ALLOYS
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
The standard Guide for the Fusion Welding of Zirconium and Zirconium Alloys provides instructional guidance for the
welding of zirconium and zirconium alloys. This guide expla... -
(PUBLIC REVIEW) C3.13M/C3.13:202X - SPECIFICATION FOR CONTROLLED ATMOSPHERE BRAZING (CAB) OF ALUMINUM
Member Price: $36.00 Non-Member Price: $48.00
This specification provides the minimum fabrication, equipment, and process procedure requirements, as well as inspection
requirements for the controlled atmosphere brazing (C... -
(PUBLIC REVIEW) C3.5M/C3.5:202X - SPECIFICATION FOR INDUCTION BRAZING
Member Price: $36.00 Non-Member Price: $48.00
This specification provides the minimum fabrication, equipment, and process procedure requirements, as well as
inspection requirements for the induction brazing of steels, cop... -
(PUBLIC REVIEW) C3.6M/C3.6:202X - SPECIFICATION FOR FURNACE BRAZING
Member Price: $36.00 Non-Member Price: $48.00
This specification provides the minimum fabrication, equipment, material, process and procedure requirements, as well
as inspection requirements for the furnace brazing of ste... -
D11.2/D11.2M:2025 - GUIDE FOR WELDING IRON CASTINGS
Formats: Printed Hard Copy, Download PDF
Member Price: $111.00 Non-Member Price: $148.00
This standard presents briefly the history and metallurgy of cast iron and the welding processes applicable to it. A weld-ability test for cast iron is described in detail and inst... -
A5.18/A5.18M:2025 - SPECIFICATION FOR CARBON STEEL ELECTRODES AND RODS FOR GAS SHIELDED ARC WELDING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for classification of carbon steel electrodes and rods, including solid, composite stranded, and composite metal cored electrodes ...
-
A4.3:2025 - STANDARD METHODS FOR DETERMINATION OF THE DIFFUSIBLE HYDROGEN CONTENT OF MARTENSITIC, BAINITIC, AND FERRITIC STEEL WELD METAL PRODUCED BY ARC WELDING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
Standard test specimens and method of preparation are set forth, along with standard methods of diffusible hydrogen analysis. The methods are suitable for shielded metal arc wel...
-
BRH:2025 BRAZING HANDBOOK, 6TH EDITION, VOL 1 FUNDAMENTALS
Formats: Printed Hard Copy, Download PDF
Member Price: $141.00 Non-Member Price: $188.00
Knowledge of the ancient art of brazing is continuously being supplemented by an ev... -
BRH:2025 BRAZING HANDBOOK, 6TH EDITION, VOL 2 PROCESSES
Formats: Printed Hard Copy, Download PDF
Member Price: $141.00 Non-Member Price: $188.00
Knowledge of the ancient art of brazing is continuously being supplemented by an eve... -
BRH:2025 BRAZING HANDBOOK, 6TH EDITION, VOL 3 MATERIALS AND APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $141.00 Non-Member Price: $188.00
Knowledge of the ancient art of brazing is continuously being supplemented by an ever-increasing amount of
technical information about metals and their behavior, so that today... -
BHCF3 - WETTING AND CAPILLARITY IN BRAZING
Member Price: $33.00 Non-Member Price: $44.00
Joining by brazing is a process in which a liquid metal, called a brazing filler metal, reacts with two or more solid metallic or ceramic parts, called base
materials. It star... -
-
-
BHCF2 - PHASE CHANGE PHENOMENA AND JOINT METALLURGY IN BRAZING
Member Price: $33.00 Non-Member Price: $44.00
-
C1.4M/C1.4:2025 - SPECIFICATION FOR RESISTANCE WELDING OF CARBON AND LOW-ALLOY STEELS
Formats: Printed Hard Copy, Download PDF
Member Price: $72.00 Non-Member Price: $96.00
This specification provides the shear strength and weld button diameter requirements ...
-
D1.3/D1.3M:2025 - STRUCTURAL WELDING CODE - SHEET STEEL
Formats: Printed Hard Copy, Download PDF
Member Price: $150.00 Non-Member Price: $200.00
This code covers the requirements associated with welding sheet steel having a minimum specified yield point no greater than 80 ksi [550 MPa]. The code requirements cover any ...
-
CCRM:2025 - D1.1 CODE CLINIC
Formats: Printed Hard Copy, Download PDF
Member Price: $150.00 Non-Member Price: $200.00
AWS Education Services publishes the AWS Code Clinic Workbook to guide and assist quality professionals – inspectors, supervisors, etc. – and quality-conscious engineers and man...
-
TWM2:2025 - TOTAL WELDING MANAGEMENT VOLUME II
Formats: Printed Hard Copy, Download PDF
Member Price: $54.00 Non-Member Price: $72.00
Throughout my many years of serving the welding industry, I developed the Total Welding Manag...
-
A5.14/A5.14M:2024 - SPECIFICATION FOR NICKEL AND NICKEL-ALLOY BARE WELDING ELECTRODES AND RODS (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
The chemical compositions of 57 nickel and nickel-alloy welding electrodes and rods are specified, including six compositions not previously classified. Major topics include genera... -
C2.21M/C2.21:2015 (R2024) SPECIFICATION FOR THERMAL SPRAY EQUIPMENT ACCEPTANCE INSPECTION
Formats: Printed Hard Copy, Download PDF
Member Price: $72.00 Non-Member Price: $96.00
This standard specifies the essential elements of a procedure for verifying the performance of thermal spray equipment to ensure it is capable of operating according to the manufac... -
D14.0/D14.0M:2024 - MACHINERY AND EQUIPMENT WELDING SPECIFICATION
Formats: Printed Hard Copy, Download PDF
Member Price: $198.00 Non-Member Price: $264.00
This specification establishes design, manufacture, quality, inspection, and repair requirements for carbon, low-alloy, and alloy steel welded connections in machinery and equipmen... -
C3.11M/C3.11:2024 SPECIFICATION FOR TORCH SOLDERING
Formats: Printed Hard Copy, Download PDF
Member Price: $66.00 Non-Member Price: $88.00
This specification describes relevant equipment, fabrication procedures, and quality (inspection) requirements for the torch soldering of materials. This document includes criteria... -
A5.21/A5.21M:2024 SPECIFICATION FOR BARE ELECTRODES AND RODS FOR SURFACING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for classification of bare (uncoated) solid wire as well as tubular electrodes and rods for weld surfacing. Solid surfacing electrode... -
A5.01M/A5.01:2019 (R2024)-WELDING AND BRAZING CONSUMABLES-PROCUREMENT OF FILLER METALS AND FLUXES
Formats: Printed Hard Copy, Download PDF
Member Price: $110.00 Non-Member Price: $110.00
This document provides a means by which the information needed for the ...
-
D17.1/D17.1M:2024 SPECIFICATION FOR FUSION WELDING FOR AEROSPACE APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $180.00 Non-Member Price: $240.00
This specification provides the general welding requirements for welding aircraft and space hardware. It includes but is not limited to the fusion welding of aluminum-based, nickel... -
A5.22/A5.22M:2024 - SPECIFICATION FOR STAINLESS STEEL FLUX CORED AND METAL CORED WELDING ELECTRODES AND RODS
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
Classification and other requirements are specified for numerous grades of flux cored and metal cored stainless steel electrodes and rods. New classifications include a duplex allo... -
A5.13/A5.13M:2024 SPECIFICATION FOR SURFACING ELECTRODES FOR SHIELDED METAL ARC WELDING
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification prescribes the requirements for classification of surfacing electrodes for shielded metal arc welding. Classification is based upon the chemical composition of t... -
C3.12M/C3.12:2024 SPECIFICATION FOR FURNACE SOLDERING
Formats: Printed Hard Copy, Download PDF
Member Price: $66.00 Non-Member Price: $88.00
This specification provides the minimum requirements for equipment, materials, processing procedures as well as inspection for metal and ceramic base materials that can be furnace ... -
D14.6/D14.6M:2024 SPECIFICATION FOR WELDING OF ROTATING ELEMENTS OF EQUIPMENT
Formats: Printed Hard Copy, Download PDF
Member Price: $87.00 Non-Member Price: $116.00
This specification establishes material and workmanship standards for manufacturers, fabricators, repair organizations, purchasers, and owner/operators of rotating equipment which ... -
D1.7/D1.7M:2024 - GUIDE FOR STRENGTHENING AND REPAIRING EXISTING STRUCTURES
Formats: Printed Hard Copy, Download PDF
Member Price: $129.00 Non-Member Price: $172.00
This guide provides information on strengthening and repairing existing structures. Included are sections on weldability,
evaluation of existing welds, testing and sampling... -
C4.9/C4.9M:2024 - RECOMMENDED PRACTICES FOR OXYACETYLENE CUTTING OF STEEL
Formats: Printed Hard Copy, Download PDF
Member Price: $105.00 Non-Member Price: $140.00
This recommended practice for oxyacetylene cutting includes general procedures to be used in conjunction with oxyacetylene
equipment and the latest safety recommendations. If ... -
A5.12M/A5.12:2024 (ISO 6848:2015 MOD) SPECIFICATION FOR TUNGSTEN AND OXIDE DISPERSED TUNGSTEN ELECTRODES FOR ARC WELDING AND CUTTING
Formats: Printed Hard Copy, Download PDF
Member Price: $110.00 Non-Member Price: $110.00
This specification prescribes the requirements for the classification of pure tungsten and oxide dispersed tungsten electrodes for gas tungsten arc welding and plasma arc welding a...
Cart